Methods to repair defects of A283GrC seamless steel pipe

When there are too many defects in the welded joints of A283GrC seamless steel pipes, welding repairs can be used for repairing. Note that the number of times of welding and repairing alloy steel at the same position is not more than 2 times, and the following regulations must be met:
1. Defects must be completely eliminated;
2. When welding A283GrC seamless steel pipes, corresponding measures need to be formulated and approved in strict accordance with the requirements of the repair process;
3. Re-appearance inspection and spectral analysis are required after rework;
4. Then heat-treat the joints of A283GrC seamless steel pipes;
5. The repair service should carry out the necessary hardness test after the heat treatment of the A283GrC seamless steel pipe;
6. After heat treatment, the reworked joint must be consistent with the original process flaw detection again.

A283GrC

The Indian government is considering revising the steel export tariff policy

Live chat

Classic Case

learn more

LEAVE A MESSAGE

We will serve you wholeheartedly, contact us through online consulting, demand table submission, e-mails, telephones, etc.

Success!
Error!
Address
Xicheng Science&Technology Building, High-tech Zone, Zhengzhou, China
Hotline
0086-371-86151827
Fax
0086-371-86011881
E-mail
sales@bebonchina.com
Live chat

Customized according to drawings

24h Technical support

Customized according to samples

24h Technical support